General Principles of Metallurgy Formulas

Ores and minerals, concentration, roasting, calcination and smelting, Ellingham diagram, reduction methods, extraction of Cu, Fe, Zn, Al, Ag and Au, and refining of metals.

13 Formulas•241+ Questions in Bank

Core Formulas & Mathematical Identities

13
01

Important Ores of Al, Fe, Cu and Zn

Al: bauxite Al2O3⋅xH2O, corundum Al2O3, cryolite Na3AlF6Fe: haematite Fe2O3, magnetite Fe3O4, siderite FeCO3, pyrites FeS2Cu: cuprite Cu2O, copper glance Cu2S, copper pyrites CuFeS2, malachite CuCO3⋅Cu(OH)2Zn: zinc blende ZnS, calamine ZnCO3, zincite ZnO\begin{array}{ll} \text{Al: bauxite } \mathrm{Al_2O_3\cdot xH_2O},\ \text{corundum } \mathrm{Al_2O_3},\ \text{cryolite } \mathrm{Na_3AlF_6} & \text{Fe: haematite } \mathrm{Fe_2O_3},\ \text{magnetite } \mathrm{Fe_3O_4},\ \text{siderite } \mathrm{FeCO_3},\ \text{pyrites } \mathrm{FeS_2} \\ \text{Cu: cuprite } \mathrm{Cu_2O},\ \text{copper glance } \mathrm{Cu_2S},\ \text{copper pyrites } \mathrm{CuFeS_2},\ \text{malachite } \mathrm{CuCO_3\cdot Cu(OH)_2} & \text{Zn: zinc blende } \mathrm{ZnS},\ \text{calamine } \mathrm{ZnCO_3},\ \text{zincite } \mathrm{ZnO} \end{array}

Ore: a mineral from which the metal can be extracted economically and profitably. Gangue (matrix) is the earthy impurity associated with the ore.

Examiner Tip: Cryolite and fluorspar are minerals of Al and Ca used as additives, not ores of Al. Azurite is 2CuCO3.Cu(OH)2 and copper pyrites is also called chalcopyrite.
02

Important Ores of Pb, Hg, Ag, Mg, Ca, Na, Sn, Mn and Cr

Pb: galena PbS, cerussite PbCO3, anglesite PbSO4Hg: cinnabar HgSAg: argentite Ag2S, horn silver AgClMg: magnesite MgCO3, carnallite KCl⋅MgCl2⋅6H2O, dolomite MgCO3⋅CaCO3Ca: limestone CaCO3, gypsum CaSO4⋅2H2O, fluorspar CaF2Sn: cassiterite SnO2,Mn: pyrolusite MnO2,Cr: chromite FeCr2O4\begin{array}{ll} \text{Pb: galena } \mathrm{PbS},\ \text{cerussite } \mathrm{PbCO_3},\ \text{anglesite } \mathrm{PbSO_4} & \text{Hg: cinnabar } \mathrm{HgS} \\ \text{Ag: argentite } \mathrm{Ag_2S},\ \text{horn silver } \mathrm{AgCl} & \text{Mg: magnesite } \mathrm{MgCO_3},\ \text{carnallite } \mathrm{KCl\cdot MgCl_2\cdot 6H_2O},\ \text{dolomite } \mathrm{MgCO_3\cdot CaCO_3} \\ \text{Ca: limestone } \mathrm{CaCO_3},\ \text{gypsum } \mathrm{CaSO_4\cdot 2H_2O},\ \text{fluorspar } \mathrm{CaF_2} & \text{Sn: cassiterite } \mathrm{SnO_2},\quad \text{Mn: pyrolusite } \mathrm{MnO_2},\quad \text{Cr: chromite } \mathrm{FeCr_2O_4} \end{array}

Names to formulas often asked directly in JEE Main. Sodium occurs as rock salt NaCl and Chile saltpetre NaNO3.

Examiner Tip: Sulphides (galena, zinc blende, copper glance, cinnabar) are concentrated by froth floatation; carbonates and hydrated oxides are calcined and sulphides are roasted.
03

Leaching: Bayer, Cyanide Process and Hydrometallurgy

Al2O3+2NaOH+3H2O→2Na[Al(OH)4]4M+8CN−+2H2O+O2→4[M(CN)2]−+4OH−2[M(CN)2]−+Zn→[Zn(CN)4]2−+2M\mathrm{Al_2O_3 + 2NaOH + 3H_2O \rightarrow 2Na[Al(OH)_4]} \quad \mathrm{4M + 8CN^- + 2H_2O + O_2 \rightarrow 4[M(CN)_2]^- + 4OH^-} \quad \mathrm{2[M(CN)_2]^- + Zn \rightarrow [Zn(CN)_4]^{2-} + 2M}

Bayer: bauxite digested in conc. NaOH at 473-523 K and 35-36 bar; Fe2O3 and TiO2 impurities do not dissolve. In the cyanide process M = Ag or Au, dissolved in aerated NaCN solution and displaced by zinc dust.

Examiner Tip: Aluminate is neutralised by CO2 gas to precipitate hydrated Al2O3, which is filtered and ignited at 1470 K to alumina. Air provides the oxidant, Zn the reducing agent; the reaction is displacement, not electrolysis.
04

Roasting, Calcination and Smelting Reactions

2ZnS+3O2→2ZnO+2SO22PbS+3O2→2PbO+2SO2ZnCO3→ZnO+CO2Fe2O3⋅xH2O→Fe2O3+xH2O\mathrm{2ZnS + 3O_2 \rightarrow 2ZnO + 2SO_2} \quad \mathrm{2PbS + 3O_2 \rightarrow 2PbO + 2SO_2} \quad \mathrm{ZnCO_3 \rightarrow ZnO + CO_2} \quad \mathrm{Fe_2O_3\cdot xH_2O \rightarrow Fe_2O_3 + xH_2O}

Roasting converts sulphides to oxides (also removes As and Sb as volatile oxides). Calcination removes CO2 and moisture from carbonates and hydrated oxides. Smelting then reduces the oxide with carbon with a flux.

Examiner Tip: Roasting: excess air, reverberatory furnace; calcination: limited or no air. Roasted ore and carbon are fused with a flux in smelting, which makes a fusible slag.
05

Reduction by Carbon, Carbon Monoxide, Aluminium and Self-Reduction

ZnO+C→ΔZn+COFe2O3+3CO→2Fe+3CO2Cr2O3+2Al→Al2O3+2Cr2Cu2O+Cu2S→6Cu+SO2\mathrm{ZnO + C \xrightarrow{\Delta} Zn + CO} \quad \mathrm{Fe_2O_3 + 3CO \rightarrow 2Fe + 3CO_2} \quad \mathrm{Cr_2O_3 + 2Al \rightarrow Al_2O_3 + 2Cr} \quad \mathrm{2Cu_2O + Cu_2S \rightarrow 6Cu + SO_2}

Reduction with C or CO is pyrometallurgy; aluminothermy (thermite, Goldschmidt) reduces Cr2O3, Mn3O4 and Fe2O3 where carbon would form carbides. Cu2O and Cu2S react among themselves in self-reduction.

Examiner Tip: Fe2O3 + 2Al thermite gives molten iron for welding rails. Aluminothermy is used for oxides of Cr, Mn which give carbides with C. HgS, PbS and Cu2S self-reduce after partial roasting.
06

Ellingham Diagram: Basis and Slope Reading

ΔG∘=ΔH∘−TΔS∘slope=d(ΔG∘)dT=−ΔS∘(per mole of O2)\Delta G^\circ = \Delta H^\circ - T\Delta S^\circ \qquad \text{slope} = \frac{d(\Delta G^\circ)}{dT} = -\Delta S^\circ \qquad (\text{per mole of } \mathrm{O_2})

Plot of ΔG° of formation of oxides (per mole of O2) against T. Most lines slope upwards because ΔS is negative (gas O2 consumed); slope changes when the metal or oxide melts or boils.

Examiner Tip: C to CO2 is almost horizontal (ΔS about 0), 2C + O2 to 2CO has a negative slope (ΔS positive, gas increases). Line for CO crosses oxide lines, so carbon reduces an oxide above the crossing temperature.
07

Thermodynamic Feasibility of Reduction

MO+C→M+CO:ΔGrxn∘=ΔG(C→CO)∘−ΔG(M→MO)∘ΔG∘=−RTln⁡K\mathrm{MO + C \rightarrow M + CO}: \quad \Delta G^\circ_{\mathrm{rxn}} = \Delta G^\circ_{(\mathrm{C \to CO})} - \Delta G^\circ_{(\mathrm{M \to MO})} \qquad \Delta G^\circ = -RT\ln K

Reduction of an oxide MO by a reducing agent is feasible when ΔG° of the overall reaction is negative, i.e. the ΔG° line of the oxide being reduced is above that of the reducing agent.

Examiner Tip: Ellingham diagram only says whether reaction is feasible thermodynamically, not how fast. Use the vertical gap at a given T: reduction is possible where the carbon line is below the metal oxide line.
08

Blast Furnace: Extraction of Iron

3Fe2O3+CO→2Fe3O4+CO2Fe3O4+4CO→3Fe+4CO2FeO+CO→Fe+CO2CaCO3→CaO+CO2CaO+SiO2→CaSiO3\mathrm{3Fe_2O_3 + CO \rightarrow 2Fe_3O_4 + CO_2} \quad \mathrm{Fe_3O_4 + 4CO \rightarrow 3Fe + 4CO_2} \quad \mathrm{FeO + CO \rightarrow Fe + CO_2} \quad \mathrm{CaCO_3 \rightarrow CaO + CO_2} \quad \mathrm{CaO + SiO_2 \rightarrow CaSiO_3}

Charge of calcined haematite, coke and limestone is fed at the top and hot air blown at the bottom. CO produced from C + O2 and CO2 + C reduces the oxides at 500-800 K (upper) and 900-1500 K (lower); CaO from limestone fuses with SiO2 to form slag.

Examiner Tip: Flux (CaO, basic) removes acidic gangue (SiO2) as slag; acidic flux (SiO2) removes basic gangue (CaO, MgO). Pig iron has about 4 percent C, cast iron about 3 percent and wrought iron is the purest at 0.1-0.25 percent C.
09

Extraction of Copper from Copper Pyrites

2CuFeS2+O2→Cu2S+2FeS+SO2FeO+SiO2→FeSiO3 (slag)2Cu2S+3O2→2Cu2O+2SO22Cu2O+Cu2S→6Cu+SO2\mathrm{2CuFeS_2 + O_2 \rightarrow Cu_2S + 2FeS + SO_2} \quad \mathrm{FeO + SiO_2 \rightarrow FeSiO_3\ (slag)} \quad \mathrm{2Cu_2S + 3O_2 \rightarrow 2Cu_2O + 2SO_2} \quad \mathrm{2Cu_2O + Cu_2S \rightarrow 6Cu + SO_2}

Roasted ore is smelted with silica: FeS is oxidised to FeO and removed as FeSiO3 slag leaving matte (Cu2S + FeS). In the Bessemer converter Cu2S is partly oxidised and self-reduces to blister copper (about 98 percent Cu).

Examiner Tip: Blister copper has a blistered surface because SO2 is released as it solidifies. Electrolytic refining: anode impure Cu, cathode pure Cu, electrolyte acidified CuSO4; Au, Ag, Pt and Sb, Se, Te collect as anode mud.
10

Hall-Heroult Process: Electrolytic Reduction of Al2O3

Cathode: Al3++3e−→AlAnode: C+O2−→CO+2e−, C+2O2−→CO2+4e−Overall: 2Al2O3+3C→4Al+3CO2\text{Cathode: } \mathrm{Al^{3+} + 3e^- \rightarrow Al} \quad \text{Anode: } \mathrm{C + O^{2-} \rightarrow CO + 2e^-},\ \mathrm{C + 2O^{2-} \rightarrow CO_2 + 4e^-} \quad \text{Overall: } \mathrm{2Al_2O_3 + 3C \rightarrow 4Al + 3CO_2}

Pure alumina in molten cryolite Na3AlF6 with CaF2 is electrolysed in an iron tank lined with carbon (cathode) using graphite anodes. Molten Al sinks to the bottom and is siphoned off.

Examiner Tip: Cryolite lowers the fusion temperature and raises the electrical conductivity. Graphite anodes are consumed (CO and CO2 evolved) and must be replaced periodically; purity of Al is about 99.8 percent.
11

Refining: Liquation, Poling, Cupellation, Distillation and Zone Refining

Liquation: Sn, Pb, BiPoling: Cu, Sn (green wood)Cupellation: Ag + PbDistillation: Zn, Hg, CdZone refining: Si, Ge, Ga, B, In\text{Liquation: Sn, Pb, Bi} \quad \text{Poling: Cu, Sn (green wood)} \quad \text{Cupellation: Ag + Pb} \quad \text{Distillation: Zn, Hg, Cd} \quad \text{Zone refining: Si, Ge, Ga, B, In}

Liquation separates low-melting metals from infusible impurities. Poling: molten blister Cu is stirred with green wood poles, whose hydrocarbon gases reduce the Cu2O impurity to Cu. Cupellation removes lead as PbO (absorbed in bone-ash cupel) from silver.

Examiner Tip: Zone refining works on the principle that impurities are more soluble in the melt than in the solid; the moving heater sweeps impurities to one end, giving ultra-pure semiconductors.
12

Vapour-Phase and Electrolytic Refining

Ni+4CO→330−350 KNi(CO)4→450−470 KNi+4COZr+2I2→ΔZrI4→1800 KZr+2I2Anode: M→Mn++ne−\mathrm{Ni + 4CO \xrightarrow{330-350\,K} Ni(CO)_4 \xrightarrow{450-470\,K} Ni + 4CO} \quad \mathrm{Zr + 2I_2 \xrightarrow{\Delta} ZrI_4 \xrightarrow{1800\,K} Zr + 2I_2} \quad \text{Anode: } \mathrm{M \rightarrow M^{n+} + ne^-}

Mond process (Ni) and van Arkel (Zr, Ti) convert the metal into a volatile compound and decompose it again. In electrolytic refining the impure metal is the anode and the pure metal the cathode in a solution of its salt.

Examiner Tip: Requirement for vapour-phase refining: metal must form a volatile compound with a reagent, and the compound should decompose easily. In electrolytic refining of Cu, less reactive impurities fall as anode mud, more reactive ones stay in solution.
13

Froth flotation

Sulphide ore + pine oil + water + air→froth\text{Sulphide ore + pine oil + water + air}\rightarrow \text{froth}

Sulphide ore particles are wetted by oil and rise; gangue is wetted by water and sinks.

Examiner Tip: NaCN is used as a depressant to separate ZnS from PbS.

Top Examiner Traps & Pitfalls

Frequently tested misconceptions in General Principles of Metallurgy

  • •Every ore is a mineral but not every mineral is an ore; an ore must allow economical extraction (clay is an Al mineral, bauxite is the Al ore).
  • •Roasting is heating in excess air (sulphide ores, gives oxide + SO2) while calcination is heating in limited or no air (carbonates and hydrated oxides); both are below the melting point of the metal.
  • •On the Ellingham diagram a metal can reduce the oxide of any metal whose line lies ABOVE its own line; the line of C to CO has a negative slope, so carbon reduces more oxides at higher temperature.
  • •In froth floatation NaCN acts as a depressant which stops ZnS from forming froth when it is mixed with PbS; it is not a collector.
  • •In the Hall-Heroult process cryolite and CaF2 are added to lower the melting point and raise conductivity; alumina is not reduced by carbon as Al lies far below the carbon lines.
  • •In the blast furnace Fe2O3 is reduced chiefly by CO (indirect reduction) in the upper part and by C near the hottest zone; limestone is the flux and forms slag CaSiO3 from silica gangue.
  • •Zinc is obtained by carbon reduction of ZnO (after roasting ZnS), not by electrolysis; its low boiling point (1180 K) lets it distil off, which also drives the reaction forward.
  • •In the Ellingham diagram a metal can reduce the oxide of any other metal lying above it.
  • •In the extraction of copper the self-reduction step has no external reducing agent.

Fundamental Theory & Core Concepts

5 Topics

1Steps in metallurgy

  • ›Concentration (hydraulic washing, magnetic separation, froth flotation, leaching) → conversion to oxide (roasting or calcination) → reduction → refining.
  • ›Reducing agents: carbon or carbon monoxide for most oxides, aluminium (thermite) for Cr₂O₃ and Mn₃O₄, electrolysis for Na, Mg, Al.
  • ›A flux combines with gangue to form a slag; an acidic gangue like SiO₂ needs a basic flux like CaO.

2Ellingham diagram

  • ›The plot of ΔG° against T for the formation of oxides shows straight lines with slope −ΔS°. Most lines slope upward because gas is consumed.
  • ›The line for 2C + O₂ → 2CO slopes downward, so carbon can reduce almost any oxide at a sufficiently high temperature.
  • ›Lines that cross show the temperature above which one element can reduce the oxide of the other.

3Concentration of ores

  • ›Hydraulic washing (gravity separation) is used when ore and gangue differ in density, e.g. oxide ores like haematite and cassiterite.
  • ›Magnetic separation is used when one of ore or gangue is magnetic, e.g. cassiterite (SnO2) from wolframite (FeWO4 and MnWO4, magnetic).
  • ›Froth floatation is used for sulphide ores: pine oil is the froth stabiliser or collector, xanthates are collectors, cresols and aniline are froth stabilisers and NaCN is a depressant.
  • ›Leaching is chemical dissolution of the ore: Al2O3 in NaOH (Bayer), Ag and Au in NaCN with air (oxidant).

4Extraction of Zn, Na and Mg

  • ›Zinc: ZnS is roasted to ZnO and reduced by heating with coke; Zn distils off as vapour because its boiling point is 1180 K.
  • ›Sodium: Down's process, electrolysis of fused NaCl with CaCl2 (lowers melting point from 1073 K) using an iron cathode and graphite anode; Na and Cl2 are collected, not the electrolyte.
  • ›Magnesium: electrolysis of fused MgCl2 (from carnallite or sea water) mixed with NaCl or CaCl2.

5Vapour-phase refining summary

  • ›Mond process for nickel: Ni + 4CO to Ni(CO)4 at 330-350 K, which decomposes at 450-470 K to pure Ni.
  • ›Van Arkel process for Zr and Ti: heated with I2 to volatile iodide, decomposed on a tungsten filament at about 1800 K.